Transient and residual stresses in a pressable glass-ceramic before and after resin-cement coating determined using profilometry.

Hdl Handle:
http://hdl.handle.net/10147/221957
Title:
Transient and residual stresses in a pressable glass-ceramic before and after resin-cement coating determined using profilometry.
Authors:
Isgró, G; Addison, O; Fleming, G J P
Affiliation:
Materials Science Unit, Division of Oral Biosciences, Dublin Dental School & Hospital, Trinity College Dublin, Lincoln Place, Dublin 2, Ireland.
Citation:
Transient and residual stresses in a pressable glass-ceramic before and after resin-cement coating determined using profilometry. 2011, 39 (5):368-75 J Dent
Journal:
Journal of dentistry
Issue Date:
May-2011
URI:
http://hdl.handle.net/10147/221957
DOI:
10.1016/j.jdent.2011.02.008
PubMed ID:
21382432
Abstract:
The effect of heat-pressing and subsequent pre-cementation (acid-etching) and resin-cementation operative techniques on the development of transient and residual stresses in different thicknesses of a lithium disilicate glass-ceramic were characterised using profilometry prior to biaxial flexure strength (BFS) determination.
Item Type:
Article
Language:
en
MeSH:
Acid Etching, Dental; Algorithms; Aluminum Oxide; Cementation; Ceramics; Dental Etching; Dental Materials; Dental Polishing; Dental Porcelain; Elastic Modulus; Hot Temperature; Humans; Hydrofluoric Acid; Materials Testing; Pliability; Resin Cements; Stress, Mechanical; Surface Properties; Time Factors
ISSN:
1879-176X

Full metadata record

DC FieldValue Language
dc.contributor.authorIsgró, Gen_GB
dc.contributor.authorAddison, Oen_GB
dc.contributor.authorFleming, G J Pen_GB
dc.date.accessioned2012-05-04T10:37:39Z-
dc.date.available2012-05-04T10:37:39Z-
dc.date.issued2011-05-
dc.identifier.citationTransient and residual stresses in a pressable glass-ceramic before and after resin-cement coating determined using profilometry. 2011, 39 (5):368-75 J Denten_GB
dc.identifier.issn1879-176X-
dc.identifier.pmid21382432-
dc.identifier.doi10.1016/j.jdent.2011.02.008-
dc.identifier.urihttp://hdl.handle.net/10147/221957-
dc.description.abstractThe effect of heat-pressing and subsequent pre-cementation (acid-etching) and resin-cementation operative techniques on the development of transient and residual stresses in different thicknesses of a lithium disilicate glass-ceramic were characterised using profilometry prior to biaxial flexure strength (BFS) determination.en_GB
dc.language.isoenen
dc.rightsArchived with thanks to Journal of dentistryen_GB
dc.subject.meshAcid Etching, Dental-
dc.subject.meshAlgorithms-
dc.subject.meshAluminum Oxide-
dc.subject.meshCementation-
dc.subject.meshCeramics-
dc.subject.meshDental Etching-
dc.subject.meshDental Materials-
dc.subject.meshDental Polishing-
dc.subject.meshDental Porcelain-
dc.subject.meshElastic Modulus-
dc.subject.meshHot Temperature-
dc.subject.meshHumans-
dc.subject.meshHydrofluoric Acid-
dc.subject.meshMaterials Testing-
dc.subject.meshPliability-
dc.subject.meshResin Cements-
dc.subject.meshStress, Mechanical-
dc.subject.meshSurface Properties-
dc.subject.meshTime Factors-
dc.titleTransient and residual stresses in a pressable glass-ceramic before and after resin-cement coating determined using profilometry.en_GB
dc.typeArticleen
dc.contributor.departmentMaterials Science Unit, Division of Oral Biosciences, Dublin Dental School & Hospital, Trinity College Dublin, Lincoln Place, Dublin 2, Ireland.en_GB
dc.identifier.journalJournal of dentistryen_GB
dc.description.provinceLeinsteren

Related articles on PubMed

All Items in Lenus, The Irish Health Repository are protected by copyright, with all rights reserved, unless otherwise indicated.