Can poly(acrylic) acid molecular weight mixtures improve the compressive fracture strength and elastic modulus of a glass-ionomer restorative?

Hdl Handle:
http://hdl.handle.net/10147/221953
Title:
Can poly(acrylic) acid molecular weight mixtures improve the compressive fracture strength and elastic modulus of a glass-ionomer restorative?
Authors:
Dowling, Adam H; Fleming, Garry J P
Affiliation:
Materials Science Unit, Division of Oral Biosciences, Dublin Dental University Hospital, Trinity College Dublin, Dublin, Ireland. adam.dowling@dental.tcd.ie
Citation:
Can poly(acrylic) acid molecular weight mixtures improve the compressive fracture strength and elastic modulus of a glass-ionomer restorative? 2011, 27 (11):1170-9 Dent Mater
Journal:
Dental materials : official publication of the Academy of Dental Materials
Issue Date:
Nov-2011
URI:
http://hdl.handle.net/10147/221953
DOI:
10.1016/j.dental.2011.08.398
PubMed ID:
21925723
Abstract:
To optimize the compressive fracture strength (σ) and elastic modulus (E) of a glass-ionomer (GI) restorative using poly(acrylic) acid (PAA) weight average molecular weight (M(w)) mixtures.
Item Type:
Article
Language:
en
MeSH:
Acrylic Resins; Analysis of Variance; Chemistry Techniques, Synthetic; Compressive Strength; Dental Restoration, Permanent; Dental Stress Analysis; Elastic Modulus; Glass Ionomer Cements; Materials Testing; Molecular Weight; Regression Analysis; Viscosity
ISSN:
1879-0097

Full metadata record

DC FieldValue Language
dc.contributor.authorDowling, Adam Hen_GB
dc.contributor.authorFleming, Garry J Pen_GB
dc.date.accessioned2012-05-04T10:27:25Z-
dc.date.available2012-05-04T10:27:25Z-
dc.date.issued2011-11-
dc.identifier.citationCan poly(acrylic) acid molecular weight mixtures improve the compressive fracture strength and elastic modulus of a glass-ionomer restorative? 2011, 27 (11):1170-9 Dent Materen_GB
dc.identifier.issn1879-0097-
dc.identifier.pmid21925723-
dc.identifier.doi10.1016/j.dental.2011.08.398-
dc.identifier.urihttp://hdl.handle.net/10147/221953-
dc.description.abstractTo optimize the compressive fracture strength (σ) and elastic modulus (E) of a glass-ionomer (GI) restorative using poly(acrylic) acid (PAA) weight average molecular weight (M(w)) mixtures.en_GB
dc.language.isoenen
dc.rightsArchived with thanks to Dental materials : official publication of the Academy of Dental Materialsen_GB
dc.subject.meshAcrylic Resins-
dc.subject.meshAnalysis of Variance-
dc.subject.meshChemistry Techniques, Synthetic-
dc.subject.meshCompressive Strength-
dc.subject.meshDental Restoration, Permanent-
dc.subject.meshDental Stress Analysis-
dc.subject.meshElastic Modulus-
dc.subject.meshGlass Ionomer Cements-
dc.subject.meshMaterials Testing-
dc.subject.meshMolecular Weight-
dc.subject.meshRegression Analysis-
dc.subject.meshViscosity-
dc.titleCan poly(acrylic) acid molecular weight mixtures improve the compressive fracture strength and elastic modulus of a glass-ionomer restorative?en_GB
dc.typeArticleen
dc.contributor.departmentMaterials Science Unit, Division of Oral Biosciences, Dublin Dental University Hospital, Trinity College Dublin, Dublin, Ireland. adam.dowling@dental.tcd.ieen_GB
dc.identifier.journalDental materials : official publication of the Academy of Dental Materialsen_GB
dc.description.provinceLeinsteren
All Items in Lenus, The Irish Health Repository are protected by copyright, with all rights reserved, unless otherwise indicated.